Titanium Ti6Al-7Nb was developed for use in the medical and surgical device applications although its properties are nearly identical to Ti6Al4V however Niobium has been substituted for Vanadium as the beta stabilizing agent giving improved biocompatability. Ti6Al7Nb is widely used in the medical device industry.

Chemical Composition Limits
Weight % Al Nb Ta Fe O C N H Ti
Titanium 6Al-7nb 5.5-6.6 6.5-7.5 0.50 max 0.25 max 0.20 max 0.08 max 0.05 max 0.009 max Bal

Product Show

Typical Mechanical Properties

Material Tensile Strength Yield Strength Elongation in 5D (%) Reduction of Area
ksi Mpa ksi Mpa
Titanium 6Al-7nb 145 1000 131 900 12 35

 

Availability
Titanium Ti6Al-7Nb is available in Bar, Rod, Wire, Rings and Forgings. For all stock and size availability contact Sales.

Forgings:
Ring size capability
OD ≤ 1300mm
Height ≤ 250mm

Disc size capability
OD ≤ 1100mm
Height ≤ 40mm

Specifications
ASTM 1295 – Bar, Rod and Wire (Annealed)
ISO 5832-11 Bar (Annealed)