Nickel Alloy/Inconel617

PRODUCTS

CONTACT US

Nickel Alloy/Inconel617

Product Description

Technical Data Sheet

Alloy 617/ Inconel 617 ® (UNS N06617) is a nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of high-temperature strength and oxidation resistance. The high nickel and chromium contents make the alloy 617 resistant to a variety of both reducing and oxidizing environments, while the aluminum with the chromium provides oxidation resistance at high temperatures. Those elements with the molybdenum enables the alloy to withstand many wet corrosive environments.

Chemical Composition Limits
Weight% Ni Cr Mo Fe S C Mn B Cu Ti Co P Si Al
Alloy 617 44.5
min
20 – 24 8 – 10 3 max 0.15
max
0.05 – 0.15 1 max 0.006 0.50
max
0.60
max
10 – 15 0.15 max 1 max 0.8 -1.5

 

Typical Mechanical Properties

Material Form Condition Yield Strength Tensile Strength Elongation % Reduction of Area Hardness, BHN
ksi MPa ksi MPa
Alloy 617 Bar Solution Annealed 46.1 318 111.5 769 56 50 181
Alloy 617 Sheet Solution Annealed 50.9 351 109.5 755 58 – 173
Alloy 617 Plate Solution Annealed 46.7 322 106.5 734 62 56 172

Product Show

Availability
Alloy 617 (Inconel 617 ®) is available in Round Bar, Flat Bar, Forging Stock, Extruded Section, Pipe, Tube, Plate, Sheet, Strip, Wire and Welding Wire. Contact Sales for further availability.

Specifications
UNS N06617
ASTM B 166
WS 2.4663a
ASME SB-166, Boiler Code Sections I, VIII,
SAE AMS 5887, SAE AMS 5888 and SAE AMS 5889
Inconel 617 ®