Cobalt Alloy 6b / Stellite 6b (AMS 5894)

PRODUCTS

CONTACT US

Cobalt Alloy 6b / Stellite 6b (AMS 5894)

Product Description

Technical Data Sheet

Cobalt alloy 6b / Stellite 6b is a cobalt-based, chromium-tungsten alloy used extensively in wear environments where its low friction coefficient minimizes the risk of seizing and galling, even in applications where lubrication is not practical. Stellite 6b is supplied in the solution treated condition (to AMS 5894) and its wear resistant properties inherent in this state limit the amount of heat treating and post machining. Typical applications for Alloy 6b include chain saw guide blades, furnace fan blades, high temperature bearings, valve stems, food processing equipment and steel mill equipment.

Chemical Composition Limits
Weight % C Mn Si P S Cr Ni Co Mo W Fe
Cobalt Alloy 6b 0.90-1.40 0.50-2.00 0.20-2.00 0.04 max 0.03 max 28.00-32.00 3.00 max bal 1.50 max 3.50-5.50 3.0 max

 

Typical Mechanical Properties  (minimums)

Material Form Tensile Strength ksi Yield Strength ksi Elongation in 4D Reduction of Area (*) Hardness (HRC)
Alloy 6b Bar (AMS 5894) 130 70 5 7 33-43
Alloy 6b Sheet / Plate (AMS 5894) 130 70 5 7 33-43
Properties shown are for sheet and plate up to 1.0″ thick and for round bar up to 3.5″ diameter.
*Reduction in area is not applicable to sheet or plate under 0.5″ thick

Product Show

Availability
Cobalt Alloy 6b / Stellite 6b is available in round bar, wire, sheet and plate. For all stock availability contact  Sales .

NEW – Aircraft Materials now offers a comprehensive range of high-quality Alloy 6 metal powders, produced and tested to exacting standards for use in all processes including Additive Manufacturing (AM), Near-Net Shape Powder Metallurgy (NNS/PS) and Hot-Isostatic Pressing (HIP).

Specifications
AMS 5894 – bar, sheet and plate
UNS R30016