Nickel Alloy 75/ Nimonic 75®

PRODUCTS

CONTACT US

Nickel Alloy 75/ Nimonic 75®

Product Description

Technical Data Sheet

Alloy 75 (UNS N06075, Nimonic 75) is a 80/20 nickel-chromium alloy with controlled additions of titanium and carbon. Nimonic 75 has good mechanical properties and oxidation resistance at high temperatures. Alloy 75 is most commonly used for sheet metal fabrications which require oxidation and scaling resistance together with medium strength at high operating temperatures. Alloy 75 (Nimonic 75) is also used in gas turbine engines, for components of industrial furnaces, for heat treating equipment and fixtures, and in nuclear engineering.

Chemical Composition Limits
Weight% Ni Cr Ti C Si Cu Fe Mn
Alloy 75
Nimonic 75
Bal 18.9 – 21.0 0.2 / 0.6 0.08 / 0.15 1.0 max 0.5 max 5.0 max 1.0 max

 

Typical Mechanical Properties

Material Test Temp °F Ultimate Tensile Strength (ksi) 0.2% Yield Strength (ksi) Elongation in 2″
Alloy 75 Sheet 1925°F Anneal Room 114.4 59.4 31
Alloy 75 Sheet 1925°F Anneal 1000 105.6 51.9 27
Alloy 75 Sheet 1925°F Anneal 1200 69.3 40.0 32
Alloy 75 Sheet 1925°F Anneal 1400 41.4 22.0 75
Alloy 75 Sheet 1925°F Anneal 1600 20.2 9.9 90
Alloy 75 Sheet 1925°F Anneal 1800 9.7 4.4 91

Product Show

Availability
Alloy 75 (Nimonic 75) is available in Bar, Round Bar, Flat Bar, Plate, Strip, Sheet, Wire,  Tube , Rod, Forging Stock and Extruded Section. For all stock availability contact Sales for further availability.

Specifications

Rod, Bar, Wire and Forging Stock BS HR 5, BS HR 504, DIN 17752, AECMA PrEN2306, AECMA PrEN2307, AECMA PrEN2306, AECMA Pr EN2307, AECMA PrEN2402, ISO 9723, ISO 9724, ISO 9725, MSRR 7004
Plate, Sheet, Strip BS HR 203, DIN 17750, AECMA PrEN2293, AECMA PrEN2302, AECMA PrEN2411, ISO 6208, MSRR 7104
Pipe and Tube BS HR 403, DIN 17751, AECMA PrEN2294, ISO 6207
Other DIN 17742, AECMA PrEN2308, Werkstoff Nr 2.4630, W. Nr 2.4951, UNS N06075, Nimonic 75 (tradename), MSRR 7104 and MSRR 7004, AFNOR NC 20T