If you need a stainless steel which offers superior strength combined with excellent oxidation resistance at elevated temperatures, then look no further than NeoNickel A286 stainless steel.
- UNS Number: S66286
- Werkstoff Number: 1.4980, 1.4943, 1.4944
- ASTM: A453, A638, 5731, 5734, 5737
- AMS: 5525, 5732, 5804, 5526
- Other: BS HR100, BS HR51, M6RR6531, 6532
-
Chemical analysis
Cr Ni Mo Co Va Al Ti B C Fe Mn Si P S Min 13.5 24 1 – 0.1 – 1.9 0.003 – – – – – – Max 16 27 1.5 1 0.5 0.35 2.35 0.01 0.08 Balance 2 Key Properties
- Density: 7.94 g/cm³
- Melting range: 1287.8 -1348.9 °C