17-4PH Stainless Steel Sheet and Plate (AMS 5604), Powder (AMS 7012)

PRODUCTS

CONTACT US

17-4PH Stainless Steel Sheet and Plate (AMS 5604), Powder (AMS 7012)

Product Description

Technical Data Sheet

17-4 PH Stainless Steel is a martensitic, precipitation-hardening stainless steel that provides an outstanding combination of high strength and hardness along with excellent corrosion resistance. 17-4 PH has good fabricating characteristics and can be age hardened by a single step, low temperature treatment. 17-4 PH is a versatile material typically used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries.

Corrosion Resistance
17-4 PH Stainless Steel withstands corrosive attack better than any of the standard hardenable stainless steels and is comparable to Type 304 in most media.

Formability
In Condition A, 17-4 PH is hard, therefore forming normally should be limited to mild operations. However, formability can be greatly improved by heat treating before cold working or by use of hot-forming methods.

Chemical Composition Limits
Weight% C Si Mn P + S max Cr Ni Cb + Ta Cu
AMS 5604 17-4PH 0.07 max 1.0 max 1.0 max 0.04 P
0.03 S
15.0 – 17.5 3.0 – 5.0 5 XC / 0.45 3.0 – 5.0

 

Typical Mechanical Properties

Material Alloy 17-4 PH Bar (AMS 5643)

Condition
Ultimate Tensile Strength (ksi) 0.2% Yield Strength (ksi) Elongation % in 2D % Reduction of Area Rockwell C Hardness
Cond A – – – – 39 max
H900 190 170 10 40 40-47
H925 170 155 10 44 38-45
H1025 155 145 12 45 34-42
H1075 145 125 13 44 31-38
H1100 140 115 14 45 30-37
H1150 135 105 16 50 28-37

Material Alloy 17-4 PH Sheet/Bar (AMS 5604)

Condition
Ultimate Tensile Strength (ksi) 0.2% Yield Strength (ksi) Elongation % in 2D (Values ​​are for sheet <0.1874″ thick) % Reduction of Area Rockwell C Hardness
Cond A – – – – 38 max
H900 190 170 5 – 40-47
H925 170 155 5 – 38-45
H1025 155 145 5 – 35-42
H1075 145 125 5 – 33-39
H1100 140 115 5 – 32-38
H1150 135 105 8 – 28-37

Product Show

Availability
17-4 PH is available in Bar, Wire, Forgings, Tube, Rings, Powder, Plate, Sheet, Strip and Welding Wire. View Stock List, Plate Stock List or contact Sales for further availability.

NEW – Aircraft Materials now offers a comprehensive range of high-quality 17-4PH metal powders, produced and tested to exacting standards for use in all processes including Additive Manufacturing (AM), Near-Net Shape Powder Metallurgy (NNS/PS) and Hot-Isostatic Pressing (HIP).

Specifications
AMS 5604 Sheet, Strip Cold Rolled and Plate.
AMS 5622 (Vac Melt) Bars (Flat, Hex, Round, Square), Wire, Forgings, Tubing and Rings
AMS 5642 Bar
AMS 5643 Bars (Flat, Hex, Round, Square), Wire, Forgings, Tubing and Rings
AMS 7012 Powder
MIL-S-25043
ASTM A564 Grade 630
ASTM A484 / ASME SA484
ASTM A564 / ASME SA564
ASTM A693 / ASME SA693 Plate, Sheet and Strip
ASTM A56 Powder
WS 1.4542
X5CrNiCuNb16-4
AFNOR Z6CNU1704
UNS S17400