Characteristics of UNS S32205
UNS S32205 has high strength and corrosion resistance at temperatures up to 316°C.
- UNS Number: S32205
- Werkstoff Number: 1.4462
- ASTM: A240, A276, A815
- Other: ASME: SA 276
Product availability
Plate
Sheet
Chemical analysis
| % | Ni | Cr | Mo | Mn | Si | C | N | S | P | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| Min | 4.5 | 22 | 3 | – | – | – | 0.14 | – | – | Balance- |
| Max | 6.5 | 23 | 3.5 | 2 | 1 | 0.03 | 0.2 | 0.02 | 0.03 | – |
Key Properties
- Density: 7.1 g/cm³
- Melting range: 1385-1443°C
- Poisson’s ration: 0.3
- Electrical resistivity: 8 x10^-7 Ωm