Titanium CP Grade 2 / AMS-T-9046 CP3 / AMS 4902

PRODUCTS

CONTACT US

Titanium CP Grade 2 / AMS-T-9046 CP3 / AMS 4902

Product Description

Technical Data Sheet

Titanium Grades 1-4 are unalloyed and generally known as CP (Commercially Pure). The tensile and yield strength of titanium generally increases with the grade number. Titanium is 30% stronger than Steel but nearly 50% lighter and although Aluminium is lighter, Titanium is stronger and has excellent strength retention. Due to Titanium’s weight, strength and high corrosion resistance it is very popular in various manufacturing industries from aerospace, medical, shipping, military etc.

Product Show

Chemical Composition Limits
Weight % Ti C Fe N O H
Titanium CP Grade 2 bal 0.08 0.30 0.05 0.020 0.015

 

Typical Mechanical Properties

Material Tensile Strength min Yield Strength Elongation (%)
ksi Mpa ksi MPa
Titanium CP Grade 2
Annealed Sheet
50 345 40-65 276-448 20
as per MIL-T-9046B, AMS-T-9046, AMS 4902

 

Availability
Titanium Grade 2 is available in Bar, Billet, Extrusion, Plate, Sheet, Strip, Wire, Pipe, Tube, Rings and Forgings. For all stock and size availability contact Sales.

Forgings:
Ring size capability
OD ≤ 1300mm
Height ≤ 250mm

Disc size capability
OD ≤ 1100mm
Height ≤ 40mm

Specifications
AMS 4902F – Sheet, strip and plate (annealed)
AMS 4941C – Tubing, welded (annealed)
AMS 4942C – Tubing, seamless (annealed)
AMS 4951F – Welding wire, commercially pure

MIL-T-9046 (TYPE 1 COMP A) CP3

BS 3TA1 – Sheet, strip
BS 2TA2 – Sheet, strip
BS 3TA3 – Bar (obsolete)
BS 2TA4 – Forgings (obsolete)
BS 2TA5 – Forgings (obsolete)

ASTM B265 Gr2 – Sheet, plate
ASTM B337 Gr2 – Pipe (withdrawn)
ASTM B338 Gr2 – Heat exchange tube
ASTM B348 Gr2 – Bar
ASTM B367 Gr2 – Castings
ASTM B381 Gr2 – Forgings
ASTM F67 Gr2 – Surgical Implant
ASTM F467 Gr2 – Nuts
ASTM F468 Gr2 – Bolts

UNS R50400
DTD 5073
AIR 9182 T40
Werkstoff WS 3.7034 (Aerospace)
Werkstoff WS 3.7035
LN 9297
DIN 17850,17860, 17862, 17863 and 17864
IMI 125
AICMA Ti-P 02
AIMS 08 -18- 002
ABS 5012

Message

Products Recommended