Titanium CP Grade 3 / AMS-T-9046 CP2/ AMS 4900

PRODUCTS

CONTACT US

Titanium CP Grade 3 / AMS-T-9046 CP2/ AMS 4900

Product Description

Technical Data Sheet

Titanium Grades 1-4 are unalloyed and generally known as CP (Commercially Pure). The tensile and yield strength of titanium generally increases with the grade number. Titanium is 30% stronger than Steel but nearly 50% lighter and although Aluminium is lighter, Titanium is stronger and has excellent strength retention. Due to Titanium’s weight, strength and high corrosion resistance it is very popular in various manufacturing industries from aerospace, medical, shipping, military etc.

Product Show

Chemical Composition Limits
Weight % Ti C Fe N O H
Titanium CP Grade 3 bal 0.08 0.30 0.05 0.30 0.015

 

Typical Mechanical Properties

Material Tensile Strength min Yield Strength Elongation (%)
ksi Mpa ksi MPa
Titanium CP Grade 3
Annealed Sheet
65 448 55-80 379-552 18
as per MIL-T-9046J, AMS-T-9046, AMS 4900

 

Availability
Titanium CP Grade 3 is available as: Bar, Billet, Extrusion, Plate, Sheet, Strip, Wire, Pipe, Tube, Rings and Forgings. For all stock and size availability contact Sales.

Forgings:
Ring size capability
OD ≤ 1300mm
Height ≤ 250mm

Disc size capability
OD ≤ 1100mm
Height ≤ 40mm

Specifications
AMS 4900 – Sheet, strip, plate
MIL-T-9046J CP2 – Sheet, strip, plate
AMS-T-9046B CP2 – Sheet, strip, plate

ASTM B265 – Gr3 Sheet, plate
ASTM B337 – Gr3 Pipe (withdrawn)
ASTM B338 – Gr3 heat exchanger tube
ASTM B348 – Gr3 bar
ASTM B367 – Gr3 castings
ASTM B381 – Gr3 forgings
ASTM F67 – Gr3 Surgical Implant
ASTM F467 – Gr3 nuts
ASTM F468 – Gr3 bolts

MSRR 8608
DTD 5023
DTD 5273
T50
Werkstoff WS3.7054
Werkstoff WS3.7055
LN 9297