Titanium Grade 5 (Ti6Al-4V) is the most commonly used alloy. Ti6Al4V is significantly stronger than other commercially pure titanium whilst still retaining the same stiffness and thermal properties (excluding thermal conductivity). Titanium Grade 5 extensively used in Aerospace, Medical, Marine and Chemical Processing.

Product Show

Chemical Composition Limits
Weight % Ti C Fe N Al O V H Y Other
Ti-6Al-4V bal 0.08 0.03 0.05 5.5-6.75 0.20 3.5-4.5 0.015 0.005 0.40

 

Typical Mechanical Properties

Material Diameter Tensile Strength min Yield Strength Elongation in 2″ Reduction of Area %
ksi Mpa ksi MPa
Titanium Alpha-Beta Ti-6Al-4V
Annealed Bar (min)
<2.00″ 135 931 125 862 10 25
Titanium Alpha-Beta Ti-6Al-4V
Annealed Bar (min)
2.00″ – 4.00″ 130 896 120 827 10 25
Titanium Alpha-Beta Ti-6Al-4V
Annealed Bar (min)
>4.00″ 130 896 120 827 8 20
as per AMS 4928

 

Material Thickness Tensile Strength Yield Strength Elongation in 2″ %
Ksi MPa Ksi MPa
Titanium Alpha-Beta Ti-6Al-4V
Annealed Sheet
0.025″ – 0.063″ 134 920 126 866 8
Titanium Alpha-Beta Ti-6Al-4V
Annealed Sheet
0.063″ – 0.1875″ 134 920 126 866 10
Titanium Alpha-Beta Ti-6Al-4V
Annealed Sheet
0.1875 – 4.00″ 130 893 120 823 10
as per MIL-T-9046J, AMS-T-9046, AMS 4911

 

Availability
Titanium 6Al4V is available in: Bar, Billet, Castings, Extrusion, Plate, Sheet, Strip, Wire,  Welding Wire , Rings and Forgings. For further stock and size information contact  Sales .

NEW – Aircraft Materials now offers a comprehensive range of high-quality Ti-6Al-4V metal powders, produced and tested to exacting standards for use in all processes including Additive Manufacturing (AM), Near-Net Shape Powder Metallurgy (NNS/PS) and Hot-Isostatic Pressing (HIP).  Find out more email us with your quality Ti-6Al-4V metal powder requirements.

Specifications

British Spec American Spec ASTM Specs European Specs
BS 3 TA10 sheet,strip
BS 3 TA11 bar
BS 2 TA12 forging stock
BS 2 TA13 forgings
BS 3 TA28  forging stock, wire
(Tensile 1100-1300MPa)
BS 2 TA56 plate
BS 2 TA59 sheet,strip
MSRR 8614
MSRR 8652
DTD 5163
DTD 5363
AMS 4907 ELI Sheet, strip, plate (annealed- ELI)
AMS 4911 Sheet, strip, plate (annealed)
AMS 4928 Bar, wire, forgings (annealed)
AMS 4930 ELI Bar, wire, forgings (annealed- ELI)
AMS 4931 ELI Bar, wire, forgings (duplex annealed- ELI)
AMS 4963 Bar, wire, forgings (modified strength)
AMS 4965 Bar, wire, forgings (solution treated & aged)
AMS 4967 Bar, wire, forgings (annealed, heat treatable)
AMS 4985 Investment castings (130ksi UTS)
AMS 4991 Investment castings (Hot Isostatic Pressed)
AMS 6931 Bar, wire, forgings (annealed)
AMS 6932 Bar, wire, forgings (annealed- ELI)AMS-T-9046 AB-1 Sheet, strip, plate (annealed)
AMS-T-9046 AB-2 (ELI) Sheet, strip, plate (annealed- ELI)
AMS-T-9047 6Al-4v Bar, wire, forgings (annealed)
AMS-T-9047 6Al-4v (ELI) Bar, wire, forgings (annealed- ELI)

MIL-T-9046J AB-1 Sheet, strip, plate (annealed)
MIL-T-9046J AB-2 (ELI) Sheet, strip, plate (annealed-ELI)
MIL-T-9046H Type 3 Comp C Sheet, strip, plate (annealed)
MIL-T-9046H Type 3 Comp D Sheet, strip, plate (annealed-ELI)
MIL-T-9047 6Al-4v Bar, wire, forgings (annealed)
MIL-T-9047 6Al-4v (ELI) Bar, wire, forgings (annealed-ELI)

ASTM Specifications
ASTM B265 Gr5 Sheet/plate
ASTM B348 Gr5 bar
ASTM B367 Gr5 castings
ASTM B381 Gr5 forgings
ASTM F136 Gr5 Implant Grade(*ground*)
ASTM F467 Gr5 nuts
ASTM F468 Gr5 bolts
ASTM F2924-14 Powder
EN 3311
ASNA 3304
ASNA 3307
DMD 776-24
DMD 774-25
WS 3.7164 (Aerospace)
WS 3.7165