Titanium CP Grade 4 / AMS-T-9046 CP1 / AMS 4901

Product Description

Technical Data Sheet

Titanium Grades 1-4 are unalloyed and generally known as CP (Commercially Pure). The tensile and yield strength of titanium generally increases with the grade number. Titanium is 30% stronger than Steel but nearly 50% lighter and although Aluminum is lighter, Titanium is stronger and has excellent strength retention. Due to Titanium’s weight, strength and high corrosion resistance it is very popular in various manufacturing industries from aerospace, medical, shipping, military etc.

Product Show

Chemical Composition Limits
Weight % Ti C Fe N O H
Titanium CP Grade 4 bal 0.08 0.50 0.05 0.40 0.015

 

Typical Mechanical Properties

Material Tensile Strength min Yield Strength Elongation (%)
ksi Mpa ksi MPa
Titanium CP Grade 4
Annealed Sheet
80 552 70-95 483-655 15
as per MIL-T-9046J, AMS-T-9046, AMS 4901

 

Availability
Titanium CP Grade 4 is available in: Bar, Billet, Extrusion, Plate, Sheet, Strip, Wire, Pipe, Forging Stock and Tube. For all stock and size availability contact  Sales .

Specifications
BS 3TA6 – Sheet, strip
BS 3TA7 – Bar
BS 2TA8 – Forging stock

AMS 4901 – Sheet, strip, plate
AMS 4921 – Bar
AMS-T-9046B – Sheet, strip, plate
AMS-T-9047A CP70 – Bar
MIL-T-9046H Type 1 Comp B – Sheet, strip, plate
MIL-T-9046J CP1 – Sheet, strip, plate
MIL-T-9074G CP70 – Bar

ASTM B265 – Gr4 Sheet, plate
ASTM B337 – Gr4 Pipe (withdrawn)
ASTM B338 – Gr4 heat exchanger tube
ASTM B348 – Gr4 bar
ASTM B367 – Gr4 castings
ASTM B381 – Gr4 forgings
ASTM F67 – Gr4 Surgical Implant
ASTM F467 – Gr4 nuts
ASTM F468 – Gr4 bolts

T-60
Werkstoff WS3.7064 (aerospace)
Werkstoff WS3.7065
LN 9297