Technical Data Sheet
Titanium Ti5Al2.5Sn (Grade 6) is a high strength alloy which is most commonly used in airframe and jet engine applications. Titanium Ti5Al2.5Sn (Grade 6) has good weldability, stability and strength at elevated temperatures.
Titanium Ti5Al2.5Sn (Grade 6) is a high strength alloy which is most commonly used in airframe and jet engine applications. Titanium Ti5Al2.5Sn (Grade 6) has good weldability, stability and strength at elevated temperatures.
| Chemical Composition Limits | |||||||||
| Weight % | Ti | C | Fe | N | Al | O | Sn | H | Other |
| Titanium Ti5Al2.5Sn | bal | 0.10 | 0.05 | 0.05 | 4.0/6.0 | 0.20 | 2.0-3.0 | 0.020 | 0.4 total max |
| Material | Tensile Strength min | Yield Strength | Elongation (%) | ||||
| ksi | Mpa | Min | Max | ||||
| ksi | Mpa | Ksi | Mpa | ||||
| Titanium Ti-5Al-2.5Sn Annealed Sheet |
120 | 830 | 115 | 795 | – | – | 10 |
Availability
Titanium Ti5Al2.5Sn is available in: Bar, Billet, Castings, Extrusion, Plate, Sheet, Wire. For all stock and size availability contact Sales.
Specifications
AMS 4926 Bars, Wire and Rings
AMS 4966 Forgings
ASTM B367 Gr6
UNS R54520
AMS 4909 Sheet, Strip, Plate (EL1 grade)
AMS 4910 Sheet, Strip, Plate
AMS 4924 Bars, Forgings, Ring (EL1 grade)
AMS 4926 Bar, Wire, Ring (Annealed – 110 ksi)
AMS 4966 Forgings
AMS 6900 Bars
AMS-T- 9046 A-1 Sheet, Strip, Plate
AMS-T- 9047 5Al-2.5Sn Bar
AMS-T-9046 A-2 (EL1) Sheet, Strip, Plate
MIL-T-9046J A-1 Sheet, Strip, Plate
MIL-T-9046H Type II Comp A Sheet, Strip, Plate
MIL-T-9046H Type II Comp B Sheet, Strip, Plate
MIL-T-9047G Bar
DTD 5083
TA14 (w/drawn)
TA15 (w/drawn)
TA16 (w/drawn)
TA17 (w/drawn)
We have been engaged in the sales of raw materials such as high-temperature alloys, corrosion-resistant alloys, precision alloys, special stainless steel materials and related product processing for more than 20 years.