Nickel Alloy X / Inconel HX ®

PRODUCTS

CONTACT US

Nickel Alloy X / Inconel HX ®

Product Description

Technical Data Sheet

Nickel Alloy X is a nickel-chromium-iron-molybdenum alloy with exceptional resistance to oxidation and outstanding strength, this alloy is used in nuclear engineering and heat treating furnaces. Nickel Alloy X is also know as Alloy HX®, Hastelloy X® and Inconel HX®.

Product Show

Chemical Composition Limits
Weight % C Cr Co Fe Mn Mo Ni Si W P S
Nicke Alloy X 0.05 – 0.15 20.5 -23 0.5 – 2.5 17.0 – 20.0 1 max 8-10 Bal 1 max 0.2 – 1.0 0.04 max 0.03 max

 

Typical Mechanical Properties

Material Condition Tensile Strength ksi Yield Strength ksi Elongation % Hardness Rb
Nickel Alloy X Sheet Annealed 115 50 45.5 90

Availability
Nickel Alloy X is available in Bar (Round), Round Bar, Flat Bar, Rod, Strip, Plate, Sheet, Wire, Pipe, Tube, Forging Stock, Powder, Extruded Section and Welding Wire. For all stock availability contact Sales.

NEW – Aircraft Materials now offers a comprehensive range of high-quality Nickel Alloy X metal powders, produced and tested to exacting standards for use in all processes including Additive Manufacturing (AM), Near-Net Shape Powder Metallurgy (NNS/PS) and Hot-Isostatic Pressing (HIP).

Specifications

Sheet AMS 5536, ASTM B435, ASME SB 435, HR204, ISO 6208, DIN 17750, AECMA PrEN2185, AIR 9165-43, LW2.4665 Part 1
Strip AMS 5536, ASTM B435, ASME SB 435, HR204, ISO 6208, DIN 17750, AECMA PrEN2185, LW2.4665 Part 1
Plate AMS 5536, ASTM B435, ASME SB 435, HR204, ISO 6208, DIN 17750, AECMA PrEN2185
Bar AMS 5754, HR6, ISO 9723, DIN 17752, AECMA PrEN2182, AIR 9165-43, LW2.4665 Part 2
Tube ASTM B775, ASTM B829, ASME SB 751, ASME SB 829, ISO 6207, DIN 17751, Welded AMS 5588, ASTM B751, ASME SB 626,Seamless AMS 5587, ASTM B622, ASME SB 622
Pipe ASTM B775, ASTM B 829, ASME SB 775, ASME SB 829, DIN 17751, Welded ASTM B619, ASME SB 619, Seamless ASTM B622, ASME SB 622
Fittings ASTM B366, ASME SB 366
Rod ASME SB 572, DIN 17752
Forgings AMS 5754, HR6, ISO 9725, DIN 17754, AECMA PrEN2182, AECMA PrEN2183, AIR 9165-43, LW2.4665 Part 2
Rings AMS 5754
Wire AMS 5798, ISO 9724, DIN 17753
Billet HR6
Powder UNS N06002
Other UNS N06002, MSRR 7158, MSRR 7127