Nickel Alloy 706/ Inconel 706®

Product Description

Technical Data Sheet

Alloy 706 (UNS N09706) is a nickel-iron-chromium. As alloy 706 is a precipitation-hardenable alloy that provides high mechanical strength in combination with good fabricability. The properties of Alloy 706 are similar to Alloy 718 however alloy 706 is more readily fabricated. The main uses of Alloy 706 are for aerospace and land base gas turbine parts and components.

Product Show

Chemical Composition Limits
Weight % Ni+Co Cr Fe Nb+Ta Ti Al C Cu Mn Si S P B Co
Alloy 706 39.0 – 44.0 14.5 – 17.5 Bal 2.5 – 3.3 1.5 -2.0 0.40 max 0.06 max 0.30 max 0.35 max 0.35 max 0.015 max 0.020 max 0.006 max 1 max

 

Typical Mechanical Properties

Material Condition Tensile Strength Ksi Yield Strength Ksi Elongation (%)
Alloy 706 Sheet
Cold Rolled
Solution Annealed 109.8 55.5 47

 

Availability
Alloy 706 (UNS N09706) is available in Round Bar and Forging Stock. For all stock availability contact Sales.

Specifications
UNS N09706
AMS 5701
AMS 5702
AMS 5703
Inconel 706 (tradename)