Titanium Alloy Grade 9 / Ti-3Al-2.5V

Product Description

Technical Data Sheet

Chemical Composition Limits
Weight % Ti C Fe N Al O V H Y Other
Titanium Ti3Al2.5V bal 0.05 0.30 0.02 2.5 / 3.5 0.12 2.0 / 3.0 0.015 0.005 0.40 total

Titanium Ti3Al2.5V (grade 9) or more simply known as Ti-3-2.5 is commonly grouped with the commercially pure grades due to it’s ability to be cold rolled. The strength of Ti3al2.5V (Ti-3-2.5) falls between Grade 4 and Grade 5 . However Ti3Al2.5V (grade 9) can be used at higher temperatures than Grade 1, Grade 2, Grade 3 and Grade 4. Applications for Ti3Al2.5V are Aerospace, Chemical Processing, Medical, Marine, Automotive industries etc.

Product Show

Typical Mechanical Properties

Material Tensile Strength min Yield Strength min Elongation (%)
ksi Mpa ksi MPa
Titanium Alpha-Beta Alloy Ti-3Al-2.5V 90 621 75 517 15
Ti-3Al-2.5V Hydraulic Seamless Tubing (annealed)

 

Availability
Titanium Ti3Al2.5V (Ti-3-2.5) is available in Bar, Tube, Strip, Coil, Sheet and Plate. For all stock and size availability contact Sales.

Specifications
ABS 5004
ABS 5141
AMS 4943 Hydraulic Seamless Tubing
AMS 4944 Hydraulic Seamless Tubing
AMS 4945 Hydraulic Seamless Tubing
B 265, ASTM B337 Gr9, ASTM B338 Gr9 & ASTM B381 Gr9
UNS R56320
AMS-T-9046 AB-5 Sheet, Strip, Plate
AMS-T-9047 3Al-2.5V Bar
MIL-T-9046J AD-5 Sheet, Strip, Plate
MIL-T-9047 3AL 2.5V Bar