Technical Data Sheet
Alloy 901 is an age-hardenable super alloy which contains Titanium and Aluminium for precipitation hardening and molybdenum for soild-solution strengthening. Alloy 901 has high yield strength and creep resistance at temperatures to about 1110°F (600°C). As Alloy 901 has a substantial iron content it enables alloy 901 to combine strength with good forging characteristics. Alloy 901 is commonly used for gas turbine engine discs, shafts, rings, casings and seals.
| Chemical Composition Limits | ||||||||||||
| Weight% | Ni | Cr | Mo | Ti | Co | Cu | Mn | Si | Al | C | S | Fe |
| Alloy 901 | 42.5 | 12.5 | 5.75 | 2.9 | 1.0 max | 0.5 max | 0.5 max | 0.4 max | 0.35 max | 0.1 max | 0.03 max | Bal |