Technical Data Sheet
Alloy PE16 is a precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. PE16 has good strength and oxidation resistance at temperature to about 1380ºF (750ºC). Alloy PE16 is designed to provide a precipitation-hardened material having excellent hot-working, cold-working and welding characteristics. PE16 is commonly used in gas-turbines components and in nuclear reactors.
| Chemical Composition Limits | |||||||
| Weight% | Ni + Co | Cr | Mo | Fe | Al | Ti | C |
| PE16 | 42-45 | 15.5-17.5 | 2.8-3.8 | Rem | 1.1-1.3 | 1.1-1.3 | 0.04-0.08 |
| Weight% | Cu | Si | Mn | Co | B | Zr | S |
| PE16 | 0.5 max | 0.5 max | 0.2 max | 2.0 max | 0.005 max | 0.02-0.04 | 0.015 max |