Technical Data Sheet
Titanium 8-1-1 (8Al-1Mo-1V) is a near alpha alloy offering good weldability and with superior creep resistance at operating temperature up to 450°C. Alloy 8-1-1 has a relatively high tensile modulus to density ratio and is used primarily in engine applications such as forged compressor blades and disks.
| Chemical Composition Limits | |||||||||
| Weight % | Al | Mo | V | Fe | C | N | H | O | Other (total) |
| Titanium 8Al-1Mo-1V |
7.35-8.35 | 0.75-1.25 | 0.75-1.25 | 0.30 | 0.08 | 0.05 | 0.015 | 0.15 | 0.40 |