Nickel Alloy 200

Product Description

Technical Data Sheet

Alloy 200 (UNS N02200) is a commercially pure wrought nickel, with good mechanical properties and an excellent resistance to many corrosive environments. Alloy 200 has good thermal, electrical and magnetostrictive properties. Alloy 201 is exactly the same but with less carbon for hotter applications. Both Alloy 200 and Alloy 201 are generally used in food processing equipment, chemical shipping drums, caustic handling equipment and piping, electronic parts, aerospace and missile components.

Product Show

Chemical Composition Limits
Weight% Ni Cu Fe Mn C Si S
Nickel Alloy 200 99.0 min 0.25 max 0.40 max 0.35 max 0.15 max 0.35 max 0.01 max
Nickel Alloy 201 99.0 min 0.25 max 0.40 max 0.35 max 0.02 max 0.35 max 0.01 max

 

Typical Mechanical Properties

Material Tensile Strength Yield Strength (0.2% Offset) Elongation in 2″ (%) Hardness
ksi MPa ksi MPa Brinnell (3000kg) Rockwell B
Nickel 200 55-75 380-520 15-30 105-210 55-40 90-120 45-70
Nickel 201 55-75 380-520 15-30 105-210 55-40 90-120 45-70

Nominal Results for Colled Rolled, Annealed Rod and Bar

Availability
Nickel 200 (UNS N02200) is available in Bar (Round bar, Flat bar), Ribbon, Wire, Rods, Tube, Pipe, Foil, Plate, Sheet, Strip and Forging Stock. For all stock availability contact Sales.

Specifications

Rod ASTM B 160, ASME SB 160, DIN 17752, ISO 9723
Bar ASTM B 160, ASME SB 160, DIN 17752, ISO 9723
Pipe ASTM B 161, ASME SB161, ASTM B 163, ASME SB 163, ASTM B 725, ASME SB 725, ASTM B 730, ASME SB 730, ASTM B 751, ASME B 751, ASTM B775, ASME SB 775, ASTM B 829, ASME SB 829 DIN 17751, ISO 6207
Tube ASTM B 161, ASME SB161, ASTM B 163, ASME SB 163, ASTM B 725, ASME SB 725, ASTM B 730, ASME SB 730, ASTM B 751, ASME B 751, ASTM B775, ASME SB 775, ASTM B 829, ASME SB 829 DIN 17751, ISO 6207
Plate ASTM B 162, ASME SB 162, DIN 17750, ISO 6208
Sheet ASTM B 162, ASME SB 162, DIN 17750, ISO 6208
Strip ASTM B 162, ASME SB 162, DIN 17750, ISO 6208
Fittings ASTM B 366, ASME SB 366
Forgings ASTM B 546, ASME SB 564, ISO 9725, DIN 17754
Wire DIN 17753, ISO 9724
Other/Similar Specs UNS N02200, UNS N02201, BS HR 10, BS 3072, BS 3073, BS 3074, BS 3075, BS 3076, NA11, Werkstoff Nr. 2.4060, 2.4066, VNI200