Nickel Alloy 600 (N06600) is a nickel-chromium-iron alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress corrosion cracking corrosion by high-purity water, and caustic corrosion. Alloy 600 also has excellent mechanical properties and has a desirable combination of high strength and good workability. Used for furnace components, in chemical and food processing, in nuclear engineering and for the sparking electrodes.

Chemical Composition Limits
Weight% C S Cr Cu Mn Si Ni Fe
Nickel Alloy 600 0.15 max 0.015 max 14.0 – 17.0 0.50 max 1.0 max 0.50 max 72.0 min 6 – 10

Typical Mechanical Properties

Material Form and Condition Tensile Strength Yield Strength Elongation % Hardness, Rockwell
ksi MPa ksi MPa
Alloy 600 rod and bar Cold drawn Annealed 80-100 550-690 25-50 170-345 55-35 65-85B
Alloy 600 Plate Hot rolled Annealed 80-100 550-725 30-50 205-345 55-35 65-85B
Alloy 600 Sheet Cold Rolled Annealed 80-100 550-690 30-45 205-310 55-35 88B max
Alloy 600 Tube and Pipe Cold Drawn Annealed 80-100 550-690 25-50 170-345 55-35 88B max
Alloy 600 Wire Cold Drawn Annealed 80-120 550-830 35-75 240-520 45-20 –
Alloy 600 Wire Cold Drawn No. 1 Temper 105-135 725-930 70-105 480-725 35-15 –
Alloy 600 Wire Spring Temper 170-220 1170-1520 150-210 1035-1450 5-2 –

Product Show

Availability
Alloy 600 is available in Pipe, Tube, Round Bar, Flat Bar, Sheet, Plate, Strip, Forging stock, Hexagon, Wire, Billet. View Stock List, Plate Stock List or contact Sales for further availability.

Specifications
UNS N06600
W. Nr 2.4816
AMS 5540 Sheet, Strip and Plate
AMS 5665 Bar, Forgings and Rings
AMS 5580 Seamless Tubing
ASTM B168 Plate
ASTM B166 Bar
ASTM B167 Seamless Pipe
ASTM B163 Seamless Tube
ASTM B517 Weld Pipe
ASTM B516 Weld Tube
ASTM B564 Forging
MIL N 22986
MIL N 23338
MIL N 6710
QQ W 390
MIL N 15721
MIL N 22987
MIL N 23229
MIL N 6840
NA14
Inconel 600 (Trademark)