Alloy 80A (Nimonic® alloy 80A) is a wrought, age-hardenable nickel-chromium alloy. Alloy 80A is similar to  alloy 75  but made precipitation hardenable by additions of aluminum and titanium. Alloy 80A has good corrosion and oxidation resistance and high tensile and creep-rupture properties at temperatures to 815ºC (1500ºF). Vacuum refined versions are also available. Alloy 80A is used for gas-turbine components (blades, rings, discs), bolts, tube supports in nuclear generators, exhaust valves in internal combustion engines and has many other offshore/marine, automotive and electrical applications.

Chemical Composition Limits
Weight % Ni Cr Ti Al C Si Cu Fe Mn Co B Zr S
Alloy 80A Bal 18.0-21.0 1.8-2.7 1.0-1.8 0.10 max 1.0 max 0.2 max 3.0 max 1.0 max 2.0 max 0.008 max 0.15 max 0.015 max

Typical Mechanical Properties

Material Condition Ultimate Tensile Strength ksi Yield Strength ksi Elongation on 4D (min) Hardness min
Alloy 80A Solution Annealed & Precipatation Treated (aged) 145 90 20 300 HV

Product Show

Availability
Alloy 80A is available in Round Bar, Flat Bar, Rod, Tube, Plate, Sheet, Strip, Forging Stock and Wire. For all stock availability contact Sales.

Specifications

Alloy 80A Rod, Bar, Wire and Forging Stock BS 3076 HR1, ASTM B 637, AECMA PrEn2188, AECMA PrEn2189, AECMA PrEn 2190, AECMA PrEn 2396, AECMA PrEn2397, AIR 9165-37
Alloy 80A Plate, Sheet and Strip BS HR 201, AECMA PrEn2191
Alloy 80A Pipe and Tube BS HR 401
Alloy 80A Other BS HR 601, BS HR1, DIN 17742, AFNOR NC 20TA, UNS N07080, Werkstoff Nr 2.4952, Werkstoff Nr 2.4631, NIMONIC 80a (trademark), MSRR 7095 and MSRR 7011, MSRR 7013, HR201, HR401, HR601, NA20, VAT80A