Technical Data Sheet
Alloy 625 (UNS N06625) is a nickel-chromium-molybdenum alloy with an addition of niobium. The addition of molybdenum acts with the niobium to stiffen the alloy matrix, providing a high strength without a strengthening heat treatment. gas, pollution control equipment and nuclear reactors.
| Chemical Composition Limits | |||||||||||||
| Weight % | Ni | Cr | Mo | Nb + Ta | Fe | Ti | C | Mn | Si | S | P | Al | Co |
| Alloy 625 | 58.0 min | 20 – 23 | 8-10 | 3.15 – 4.15 | 5.0 max | 0.40 max | 0.10 max | 0.50 max | 0.50 max | 0.15 max | 0.15 max | 0.40 max | 1.0 max |
Typical Mechanical Properties
| Material | Form and Condition | Tensile Strength MPa | Yield Strength (0.2% Offset) MPa | Elongation 4D (%) | Hardness HB | ||
| Ksi | MPa | Ksi | MPa | ||||
| Alloy 625 Bar | Annealed | 120 | 827 | 60 | 414 | 30 | ≤ 287 HB |
| Alloy 625 Sheet | Annealed | 120 | 827 | 60 | 414 | 30 | 145-240 |
| Alloy 625 Tube Seamless and Welded |
Annealed | 120 | 827 | 60 | 414 | 35 | – |