BS 3 TA10 sheet,strip
BS 3 TA11 bar
BS 2 TA12 forging stock
BS 2 TA13 forgings
BS 3 TA28 forging stock, wire
(Tensile 1100-1300MPa)
BS 2 TA56 plate
BS 2 TA59 sheet,strip
MSRR 8614
MSRR 8652
DTD 5163
DTD 5363 |
AMS 4907 ELI Sheet, strip, plate (annealed- ELI)
AMS 4911 Sheet, strip, plate (annealed)
AMS 4928 Bar, wire, forgings (annealed)
AMS 4930 ELI Bar, wire, forgings (annealed- ELI)
AMS 4931 ELI Bar, wire, forgings (duplex annealed- ELI)
AMS 4963 Bar, wire, forgings (modified strength)
AMS 4965 Bar, wire, forgings (solution treated & aged)
AMS 4967 Bar, wire, forgings (annealed, heat treatable)
AMS 4985 Investment castings (130ksi UTS)
AMS 4991 Investment castings (Hot Isostatic Pressed)
AMS 6931 Bar, wire, forgings (annealed)
AMS 6932 Bar, wire, forgings (annealed- ELI)AMS-T-9046 AB-1 Sheet, strip, plate (annealed)
AMS-T-9046 AB-2 (ELI) Sheet, strip, plate (annealed- ELI)
AMS-T-9047 6Al-4v Bar, wire, forgings (annealed)
AMS-T-9047 6Al-4v (ELI) Bar, wire, forgings (annealed- ELI)
MIL-T-9046J AB-1 Sheet, strip, plate (annealed)
MIL-T-9046J AB-2 (ELI) Sheet, strip, plate (annealed-ELI)
MIL-T-9046H Type 3 Comp C Sheet, strip, plate (annealed)
MIL-T-9046H Type 3 Comp D Sheet, strip, plate (annealed-ELI)
MIL-T-9047 6Al-4v Bar, wire, forgings (annealed)
MIL-T-9047 6Al-4v (ELI) Bar, wire, forgings (annealed-ELI) |
ASTM Specifications
ASTM B265 Gr5 Sheet/plate
ASTM B348 Gr5 bar
ASTM B367 Gr5 castings
ASTM B381 Gr5 forgings
ASTM F136 Gr5 Implant Grade(*ground*)
ASTM F467 Gr5 nuts
ASTM F468 Gr5 bolts
ASTM F2924-14 Powder |
EN 3311
ASNA 3304
ASNA 3307
DMD 776-24
DMD 774-25
WS 3.7164 (Aerospace)
WS 3.7165 |