| Chemical Composition Limits |
| Weight % |
Ti |
C |
Fe |
N |
O |
H |
| Titanium CP Grade 2 |
bal |
0.08 |
0.30 |
0.05 |
0.020 |
0.015 |
Typical Mechanical Properties
| Material |
Tensile Strength min |
Yield Strength |
Elongation (%) |
| ksi |
Mpa |
ksi |
MPa |
Titanium CP Grade 2
Annealed Sheet |
50 |
345 |
40-65 |
276-448 |
20 |
| as per MIL-T-9046B, AMS-T-9046, AMS 4902 |
Availability
Titanium Grade 2 is available in Bar, Billet, Extrusion, Plate, Sheet, Strip, Wire, Pipe, Tube, Rings and Forgings. For all stock and size availability contact Sales.
Forgings:
Ring size capability
OD ≤ 1300mm
Height ≤ 250mm
Disc size capability
OD ≤ 1100mm
Height ≤ 40mm
Specifications
AMS 4902F – Sheet, strip and plate (annealed)
AMS 4941C – Tubing, welded (annealed)
AMS 4942C – Tubing, seamless (annealed)
AMS 4951F – Welding wire, commercially pure
MIL-T-9046 (TYPE 1 COMP A) CP3
BS 3TA1 – Sheet, strip
BS 2TA2 – Sheet, strip
BS 3TA3 – Bar (obsolete)
BS 2TA4 – Forgings (obsolete)
BS 2TA5 – Forgings (obsolete)
ASTM B265 Gr2 – Sheet, plate
ASTM B337 Gr2 – Pipe (withdrawn)
ASTM B338 Gr2 – Heat exchange tube
ASTM B348 Gr2 – Bar
ASTM B367 Gr2 – Castings
ASTM B381 Gr2 – Forgings
ASTM F67 Gr2 – Surgical Implant
ASTM F467 Gr2 – Nuts
ASTM F468 Gr2 – Bolts
UNS R50400
DTD 5073
AIR 9182 T40
Werkstoff WS 3.7034 (Aerospace)
Werkstoff WS 3.7035
LN 9297
DIN 17850,17860, 17862, 17863 and 17864
IMI 125
AICMA Ti-P 02
AIMS 08 -18- 002
ABS 5012