Product Description

Characteristics of UNS S32205

UNS S32205 has high strength and corrosion resistance at temperatures up to 316°C.

  • UNS Number: S32205
  • Werkstoff Number: 1.4462
  • ASTM: A240, A276, A815
  • Other: ASME: SA 276

Product availability

Plate
Sheet

Chemical analysis

% Ni Cr Mo Mn Si C N S P Fe
Min 4.5 22 3 – – – 0.14 – – Balance-
Max 6.5 23 3.5 2 1 0.03 0.2 0.02 0.03 –

Key Properties

  • Density: 7.1 g/cm³
  • Melting range: 1385-1443°C
  • Poisson’s ration: 0.3
  • Electrical resistivity: 8 x10^-7 Ωm

Product Show

About UNS S32205

UNS S32205 is a duplex grade with a ferritic-austenitic microstructure. The alloy consists of around 40-50% ferrite in the annealed condition. The duplex microstructure has the high strength of the ferritic grades whilst retaining the corrosion resistance of the austenitic grades.

UNS S32205 has superior resistance to chloride pitting and crevice corrosion as compared to 317L stainless steel. The alloy has outstanding corrosion resistance to seawater and most concentrations of sulfuric acid. In addition, UNS S32205 duplex stainless is also resistant to sulphide stress corrosion cracking (sour-gas environments).

The high quality and therefore performance of UNS S32205 is widely attributed to the high levels of chromium present as well as nitrogen and molybdenum.

To learn more about UNS S32205 contact us, or fill in our online quote form and we’ll get right back to you!

Mechanical & Physical Properties

Mechanical & Physical Properties 21.1°C 100°C 200°C 300°C
Coefficient of Thermal Expansion µm/m⁰C 14.4 14.4 14.4
Thermal Conductivity/kcal/(hr.m.°C) 11.9 13.4 14.9 16.4
Modulus of Elasticity/ x10 5  MPa 1.93 1.79 1.72 1.65

Mechanical Specified Properties, ASTM A240

95 Ultimate Tensile Strength, ksi
65 0.2% Yield Strength, ksi
25 Elongation, %
290 Hardness MAX, Brinell

Corrosion Resistance

Alloy PREN Critical Pitting Temperature, CPT
2205 34 130°F
316L twenty four 62°F